Go to Main text Go to Main Menu

TRILOY® 210GNH20

PC/ABS

Inquiry

TYPICAL DATA OF TRILOY® 210GNH20 GRADE

PROPERTY UNIT ASTM METHOD TYPICAL DATA
Physical
Specific Gravity - D792 1.31
Water Absorption (24 hours at 23℃) % D570 0.2
Melt Flow Rate (260℃, 2.16kg) g/10min D1238 36
MECHANICAL
Tensile Strength at yield kgf/㎠ D638 1,000
Tensile Elongation at break % D638 2
Flexural Strength at yield kgf/㎠ D790 1,200
Flexural Modulus kgf/㎠ D790 60,000
Izod Impact Strength, notched, 23℃ (1/8”) kgf∙㎝/㎝ D256 6
Rockwell Hardness R scale D785 121
THERMAL
HDT, 18.6 ㎏f/㎠ D648 88
ELECTRICAL
OTHERS
UL-94 Flammability (1.4mm thickness) - (UL 94) V-0
Mold Shrinkage (3mm thickness) % D955 0.2~0.4
※The figures listed in this table are typical values obtained under the standard test methods and may not be applicable for products that are under different application condition.

PROCESSING GUIDE FOR TRILOY® 210GNH20 GRADE

General processing conditions for TRILOY® 210GNH20 are shown below.
Drying prior to processing is essential to ensure desired appearance and property performance.

SPECIFICATION UNIT CONDITIONS
Drying Temperature 75~85
Drying Time hr 3~5
Moisture Content, Max % 0.02
Melt Temperature 260~280
Nozzle Temperature 250~290
Front Temperature 260~280
Middle Temperature 260~290
Rear Temperature 260~280
Mold Temperature 40~90