PROPERTY UNIT ASTM METHOD TYPICAL DATA
Physical
Specific Gravity - D792 1.09
MECHANICAL
Tensile Strength at yield kgf/㎠ D638 1,150
Flexural Strength at yield kgf/㎠ D790 1,550
Flexural Modulus kgf/㎠ D790 65,000
Izod Impact Strength, notched, 23℃ (1/8”) kgf∙㎝/㎝ D256 18.5
THERMAL
HDT, 4.6 ㎏f/㎠ 160
ELECTRICAL
OTHERS
Mold Shrinkage (3mm thickness) % D955 0.25~0.4
※The figures listed in this table are typical values obtained under the standard test methods and may not be applicable for products that are under different application condition.

PROCESSING GUIDE FOR TRILFT® LF9080G30 GRADE

General processing conditions for TRILFT® LF9080G30 are shown below.
Drying prior to processing is essential to ensure desired appearance and property performance.

SPECIFICATION UNIT CONDITIONS
Drying Temperature 80~100
Drying Time hr 3~5
Moisture Content, Max % 0.02
Melt Temperature 220~240
Nozzle Temperature 230~240
Front Temperature 220~230
Middle Temperature 220~230
Rear Temperature 210~220
Mold Temperature 40
Screw Speed rpm <50
Vent Depth mm 0.02~0.05