TYPICAL DATA OF TRILOY® DM280P GRADE

PROPERTY UNIT ASTM METHOD TYPICAL DATA
Physical
Specific Gravity - D792 1.32
Water Absorption (24 hours at 23℃) % D570 0.2
Melt Flow Rate (260℃, 2.16kg) g/10min D1238 28
MECHANICAL
Tensile Strength at yield kgf/㎠ D638 500
Tensile Elongation at break % D638 5
Flexural Strength at yield kgf/㎠ D790 850
Flexural Modulus kgf/㎠ D790 42,000
Izod Impact Strength, notched, 23℃ (1/8”) kgf∙㎝/㎝ D256 4.5
THERMAL
HDT, 18.6 ㎏f/㎠ D648 85
ELECTRICAL
OTHERS
UL-94 Flammability (1.0mm thickness) - (UL 94) V-0
UL-94 Flammability (2.0mm thickness) V-0, 5VB
Mold Shrinkage (3mm thickness) % D955 0.2~0.4
※The figures listed in this table are typical values obtained under the standard test methods and may not be applicable for products that are under different application condition.

PROCESSING GUIDE FOR TRILOY® DM280P GRADE

General processing conditions for TRILOY® DM280P are shown below.
Drying prior to processing is essential to ensure desired appearance and property performance.

SPECIFICATION UNIT CONDITIONS
Drying Temperature 80
Drying Time hr 3~5
Moisture Content, Max % 0.02
Melt Temperature 250~280
Nozzle Temperature 240~270
Front Temperature 245~265
Middle Temperature 245~265
Rear Temperature 235~265
Mold Temperature 60~90